PROTECT AC 775

DEFINITION

Two component solvented epoxy lacquer.

USAGE AREAS

It is used on wood, concrete, natural stone, and metal surfaces.

 

Type

 

TS EN 1504-2/ April 2008 Principle 5(PR): 5.1 Physical Resistance / Surface Improvement Coating Application (C)

Colour

Transparent

Outlook

Bright

Thinner

Epoxy Thinner

Solid Matter by Weight, %

40

Density

1,0 g/cm³

Waste

For 30 micron tickness at one coat 80 gr/m²

Package

14 kg A Component + 7 kg B Component:Total 21 kg

Flash Point

>25 °C

Mixture Ratio

2 / 1

Application Methods

Brush, Roller, Air Gun, Airless Gun

Mixture Life

1 hour / 25°C

Shelf Life

1 year

Waiting Time Between Coats

6 hours/ 25°C

Drying Time

12 hours/ 25°C

Mechanical Strength

7 days

Equipment Cleaning

Epoxy Thinner

SURFACE PREPARATION

The surfaces to be applied should be cleaned with acetone and free from oil and dust.

MIXING PREPARATION

A and B component should be mixed with a low speed mixer for at least 3-4 minutes until a homogenous mixture is obtained by paying attention to mixture ratios. It is ready for application after mixing.

APPLICATION CONDITIONS

Avoid application in very humid environments and below 10°C