FUGAPOX SC 380

DEFINITION

Two component, solvent free, high strength, chemical resistant, hygienic epoxy joint filler and ceramic adhesive for humidy surfaces. .

USAGE AREAS

It is used in concrete, natural stone, aerated concrete, ceramic, pools, food facilities, restoration of historical buildings, filling of corner, crack dilation holes and cracks, where chemical resistance is required. It can also be used on vertical surfaces.

Type

TS EN 12004 ( system 3)

Colour

White

Outlook

Matt

Solid Matter by Weight, %

99

Density

1,80 gr/cm³

Waste

Look at the waste table

Package

4,50 kg A Component + 1,50 kg B Component: Total 6 kg

Flash Point

>25 °C

Mixture Ratio

3 / 1

Application Methods

Trowel, Scraper

Mixture Life

50 minutes/ 25°C

Shelf Life

1 year

Waiting Time Between Coats

12 hours / 25°C

Drying Time

12 hours / 25°C

Bending Strength

Adhesion Strength (To steel)

Breakage from concrete

Pressure Strength

20 ºC de min. 28 N/mm² (7 days )

6,50 N/mm² (7 days )

3,50 N/mm² (7 days )

20 ºC de min. 28 N/mm² (7 days )

SURFACE PREPARATION

The surfaces must be free from oil and dirty.

MIXING PREPARATION

A and B component should be mixed with a low speed mixer for at least 3-4 minutes until a homogenous mixture is obtained by paying attention to mixture ratios. It is ready for application after mixing.

APPLICATION CONDITIONS

* Avoid application below 10°C.

* Mixing ratios should be considered.

* The excess material adhered to the ceramic or faience should be cleaned with hot water without waiting drying.