EPOKSİ ÜRÜNLER
-
Floor Coatings
- PRIMER WG 032
- WALL WG 034
- BRV SC 105
- BRV SC-200 K
- PRIMER SC 210
- PRIMER SC 215
- PRIMER SC 220
- SC Z-230
- PRIMER SC 270
- PRIMER SC 325
- DECOFLOOR SC 330
- FLOOR SC 470
- SC 600
- WALL SC 605
- WALL SC 605-C
- BRV SC 610 SOLVENTSİZ EPOKSİ SON KAT BOYA-ENG
- BRV SC 620 SOLVENTSİZ TEKSTÜRLÜ EPOKSİ SON KAT BOYA-E
- BRV SC 625 SOLVENTSİZ EPOKSİ SON KAT KAYMAZ ZEMİN BOYASI-E
- FLOOR SC 645
- SC 650 ST
- FLOOR SC 902
- FLOOR SC 903
- BRV SC 905 • DÜŞEY YÜZEYLER İÇİN KİMYASAL MADDELERE DAYANIKLI SOLVENTSİZ EPOKSİ SON KAT BOYA
- FLOOR SC 950
- FLOOR SC 1200
- FLOOR AC 6380
- ROAD AC 6388
- Waterproofing Products
- Repair Anchorage and Assembly Products
- Joint Filler and Ceramic Adhesive Products
- Wood Protection Adhesive and Lamination Products
- Natural Stone Protectors
- Water Reservoir & Drainpipe Insulation Products
- Anticorrosive Products For Metal Surfaces
- Thinners
-
Floor Coatings
-
POLIURETAN PRODUCTS
- ZEMIN KAPLAMA ve BOYAMA URUNLERI
- SU YALITIM URUNLERI
- YAPISAL GUCLENDIRME TAMIR ANKRAJ MONTAJ URUNLERI
- AHSAP KORUYUCU, YAPISTIRICI ve LAMINASYON URUNLERI
- DOGALTAS KORUYUCU URUNLER
- METAL YUZEYLER ICIN ANTIKOROZIF URUNLER
- Concrete Protection and Shining Products
- TINERLER
-
AKRILIK PRODUCTS
- SU YALITIM URUNLERI
- ZEMIN KAPLAMA ve BOYAMA URUNLERI
- Indoor & Outdoor Insulation and Painting
- Fire Retardant Insulation Paint
BRV SC 102
DEFINITION
PRODUCT DESCRIPTION
Two component, solvent free epoxy wooden adhesive
USAGE AREAS
It is used for adhering wood to concrete, wood to wood, wood to metal and for lamination of wood. PRIMER SC 102 also exhibits adhesion performance on moist surfaces
Type | TS EN 12004 (system 3) |
Colour | Blurred |
Outlook | Mat |
Solid Matter by Weight, % | 100 |
Density | 1,20 gr/cm³ |
Waste | 0,400 – 0,600 kg / m2 |
Package | 15 kg A Component + 15 kg B Component:Total 30 kg |
Flash Point | >25 °C |
Mixture Ratio | 1 / 1 |
Application Methods | Brush, Roller, Trowell |
Mixture Life | 30 minutes / 25 °C |
Shelf Life | 1 yeat |
Waiting Time Between Coats | 12 hours / 25 °C |
Drying Time | 12 hours / 25 °C |
Mechanical Strength | 7 days |
Equipment Cleaning | Epoxy Thinner |
SURFACE PREPARATION
The surfaces are abraded with 80-120 sand sandpaper, Cleaned with thinner. The oiled trees should be thoroughly wiped with acetone before being bonded. The evaporation of the solvent should be allowed without going to the bonding process. If laminating is to be done on the concrete, the surface should be roughened with blastrac or diamond grainder and after priming SC 092 Epoxy adhesion bridge primer with prime, lamination should be started.
MIXING PREPARATION
A and B component should be mixed with a low speed mixer for at least 3-4 minutes until a homogenous mixture is obtained by paying attention to mixture ratios. It is ready for application after mixing.
APPLICATION CONDITIONS
* Avoid application below 10°C.
* Mixing ratio should be considered.
* SC 102 Epoxy Wood Adhesive adheres almost all materials prepared directly except thermoplastics such as PVC and polypropylene. Do not use on GRP surfaces that are not fully cured.
USAGE METHOD
WOOD LAMINATION
The SC 092 Epoxy Adhesive Bridge, a wood preservative, is used to enhance resistance to wood-destroying microorganisms. SC 092 Epoxy Adhesion Bridge is applied by brush or roller. SC 102 Epoxy Wood Adhesive is applied to wood parts with a brush or roller, and if there are deep gaps in the wood, MRN 740 Microfiber can be added to increase the consistency of the product. Wood parts are bonded one by one with bench clamps. Bench clamps can be opened at 25 ° C in 5-12 hours
WOODEN PLYWOOD LAMINATION
The SC 092 Epoxy Adhesive Bridge, a wood preservative, is used to increase resistance to wood-destroying microorganisms. SC 092 Epoxy Adhesion Bridge is applied enough by brush or roller. For applications that last 24 hours (25°C), the surface should be roughened with appropriate sandpaper and cleaned with acetone. In the application of plywood lamination, a mixture of SC 102 Epoxy Wood Adhesive is applied to the surface enough, MRN 740 Microfiber can be added to increase the consistency of the product if there are deep gaps in the wood. The pieces of plywood lamination are fixed to the lamination surface with individual plastic punches. For applications that last 24 hours (at 25 ° C), they should be roughened with appropriate sandpaper and cleaned with acetone