POWER CONCRETE LITHIUM GUARD

DEFINITION

Colour

Transparent

Outlook

Bright

Thinner

Ready to use

Solid Matter by Weight, %

16

Density

Surface penetration

1,1 gr/cm3

2-8 mm

Waste

Between  100 gr – 250 gr/m2 at single coat depending on the roughness and suction condition of the application surface.

Package

5, 10, 20 kg in plastic bins

Application Methods

Brush, roller, air or airless gun

Application Temperature

It should be applied at temperatures above 10 ºC..

Shelf Life

1 yıl

Drying Time

Waiting time between coats

1-2 hours /25 °C

10-15 minutes without product deposit (wet damp appearance

Equipment Cleaning

Water

SURFACE PREPARATION

The surface must be cleaned from oil, dirt, rust, dust and all kinds of residues. Acid-containing cleaners should not use since it will degrade the surface properties of the concrete floor to be applied.

* Easy to apply.

* High penetration ability (2-8 mm from surface 2-8 mm)

* Water based.

* Nano Technological structure and containing sodium silicate.

* Maximum dust tolerance on concrete surfaces

* Creates shiny and mechanical strength, a high concrete surface.

* Prevents salt vomit, flowering and staining.

* It would be a very good penetrating into concrete it reacts with the lime in the concrete structure and forms a bond which is insoluble in the concrete.

* Allows the concrete surface to breathe.

* Maintenance and cleaning is easy.

* Extends the life of concrete.

*No harm to the environment and human health due to low VOC content.