General Details

DEFINITION

Two component, high mechanical and chemical resistance, high tensile and tear strength, resistant to -30ºC, solvent free, polyurethane self leveling coating

USAGE AREAS

It is used as elastic polyurethane floor covering at hospitals, schools, offices, sports halls, shopping centers, hotels, storage areas, cold storage, in the frigofric vehicle chassis, in food production facilities and in all industrial areas where hygiene is

Product Features
Type TS EN 1504-2/ April 2008 Principle 5 (PR): 5.1 Physical Resistance / Surface Improvement Coating Application (C)
Colour RAL colours
Outlook Semi Bright
There may be discoloration in environments exposed to direct sunlight, but it does not negatively affect the performance of the product.
Solid Matter by Weight, % 100
Density A+B 1,20 gr/cm³
A+B+C 1,40 gr/cm³
Waste For 1 mm dry film thickness A+B  1,200 kg / m²
For 1 mm dry film thickness A+B+C 1,400 kg/m²
Package Component A:16 kg  Component B:4 kg Total: 20 kg
Component A:16 kg Component B: 4 kg Component C:12,5 kg Total.32,5 kg
Component C is in 25 kg Kraft Bag packaging
Flash Point >25 °C
Mixture Ratio 4 / 1
Application Methods Brush, Roller, Trowel
Mixture Life 30 minutes /25 °C
Shelf Life 1 year
Waiting Time Between Coats 8 hours/25 °C
Drying Time 8 hours/25 °C
Mechanical Strength 7 days
Shore A Hardness (7 days / 25°C)

Wear Resistance (TABER)
Capillary Water Absorption and Water Permeability
Resistance to impact
Break on Tensile
Fire Response Class

75
223 mg TS 8103 EN ISO 5470-1:2002
0,001 (kg/m².h ) TS EN 1062-3:2008
Sınıf ll TS EN ISO 6272-1:2006
5 (N/mm²) TS EN 1542:2001
Efl
Equipment Cleaning Polyurethane Thinner

 

Implementation

SURFACE PREPARATION

* Prior to applying the primer coat, the surfaces to be applied must be free from oil, dust, and dirty.

* Free parts on the surface, cement grout on concrete surfaces and parts that prevent adhesion must be cleaned.

MIXING PREPARATION
A and B component should be mixed with a low speed mixer for at least 3-4 minutes until a homogenous mixture is obtained by paying attention to mixture ratios. It is ready for application after mixing. The mixture should be consumed within 25-30 minutes.